Wednesday, December 28, 2022

Re: [MW:33878] Low alloy vs high alloy steel

Dear Mr. Mithlesh kumar,

when we adding the total alloying elements of Cr,Ni,Mo, if the total is less than or equal to 10% this is low alloy steel, total alloys are greater than 10 % that is high alloy steel.

A335 P9 - low alloy steel pipe.     

Regards,
Sankaran.SP
Welding & Metallurgy expert
Coimbatore, India. 


On Wednesday, 28 December, 2022 at 11:53:51 am IST, mithlesh kumar <mithleshmech47@gmail.com> wrote:


Dear expert ,

Please brief difference between low alloy steel vs high alloy steel.

A335 P9 is low or high alloy steel.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/62edc733-0051-4b57-9c08-171a8ff85d71n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...