Dear sir,
          I have one clarification for ELECTRODE QUALIFICATION TEST. OUR PROJECT USING BOTH E6010 AND E8010.PLEASE CLARIFY NEED SEPAPATE TEST FOR E6010 AND E8010 OR ONE TEST FOR BOTH ELECTRODE.PLEASE SIR
   Thanks and regards,

     S.KARUNAKARAN,
      karunaqc@gmail.com
      91-6382279754
      91-7826930029(Whats app).







On Fri, Dec 23, 2022 at 9:51 AM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
usability is same except strength

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, Dec 23, 2022 at 9:26 AM Karunakaran Karan <karunaqc@gmail.com> wrote:
Dear Sir.
   Any have TQ for above subject please share me. My site using E8010 .but Site document mention E7070.so I need TQ for Using E8010.
Thank you

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHt4qw8uFh0UP%2BruTnOPTF7LHjMUWEuzSzeuavfcq%3DOUEHgFTg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNSKz8DON3Y47Jc4GDW4icB25wMNR15Z77F%3D3W%2BtmBaNw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHt4qw_6a%2BvR1VngesJYCG9vsHMcQ9wyTXKmL3j05%3D9JdZn3FQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...