Re: [MW:32432] Welding after PWHT and Hydrotest

Pl read PW 54 in detail.

On Sat, 26 Jun 2021, 16:07 Manish Kumar, <mkmkr431@gmail.com> wrote:
Dear Sir,
As per ASME section 1, What Can be allowed Welding on weld zone and shell of vessel after Heat treatment and PWHT ?

Please advise as per ASME section 1.



Regards
Manish Kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k7Uhb32jRhPjyossp4wwW_E03Ef09cAjD0fUhz08fQt1g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3MigKEuOKDvf41JoZSjo22EeZX9%2BYw%3D8RxCXJ55Bop_hw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...