Re: [MW:32421] Welding Electrode Selection Table

Thank you so much for your effort taken to write me a adequate information. I feel good and thankful Mr. Gerald. All the best. 

Best Regards,

Venkat G

On Fri, 4 Jun 2021 at 5:12 AM, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Thanks  Mr. Venkatachalam,

The details provided by me gives only a guideline for selecting appropriate welding consumable based on suitability and matching chemical composition.

Apart from this there are various API, NACE, NiDL, SSA, Client specification and various Technical Articles which must be considered apart from the recommendation of ASME Sec.IIC based on Application such as Refinery, Natural Gas Plants, Petrochemical plants, Fertilizer plants etc. for Equipment and piping. It is always better to consult a Welding Engineer or Welding consultant/

Thanks & Regards

J.Gerald Jayakumar



On Thursday, 3 June, 2021, 05:32:15 pm IST, Venkatachalam Govindan <vinisaa@gmail.com> wrote:


Thank you so much, dear, Gerald, for considering my request. All the best.

Venkat G.

On Thu, 3 Jun 2021 at 9:48 AM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Mr.Venkatachalam,

Please refer to API RP 582.

Please also refer the below link.


Snap shot of the link below.




Thanks & Regards

J.Gerald Jayakumar



On Wednesday, 2 June, 2021, 05:55:23 pm IST, Venkatachalam Govindan <vinisaa@gmail.com> wrote:


Dear Respected Professionals, Gday.

We need a welding rod selection table, or suitable comparison table or the proper reference to select the electrode to any particular material if required. Hope our friends will help me. Thank you. All the best. 

Best Regards,
--
Venkatachalam Govindan
QHSE Lead | Auditor | Trainer
(API U Trainer | IRCA Lead Auditor | Exemplar Global MS Specialist |CQI Practitioner)
Mobile +965-97604989

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHOK3OdqswNz6gvYtwT%2BUY%3DckN5MC%2BbqhzOMF-zMSqidvwXL-w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1994280717.1679549.1622702087899%40mail.yahoo.com.


--
Venkatachalam Govindan
QHSE Lead | Auditor | Trainer
(API U Trainer | IRCA Lead Auditor | Exemplar Global MS Specialist | CQI Practitioner)
Mobile +965-97604989

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2020800168.1716922.1622724206792%40mail.yahoo.com.
--
--
Venkatachalam Govindan
Auditing & Training Manager
IRCA Registered Lead Auditor | API U Trainer |
CQI Practitioner | Exemplar Global CMSS
Kuwait +965-97604989 India +91-9840502376

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHOK3OdwW39ckXmr-1dJW33-p%2By8CWBmji_BrMaX4stmj95aPw%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...