Re: [MW:32426] Regarding Impact testing for pipe supports.

Remove one support and do all physical testing .
Discuss with Clinet about this action and take concent.

On Wed, 23 Jun 2021, 11:18 mohit aggarwal, <aggarwalmoh@gmail.com> wrote:
PMI will be carried out but what about base material. Main problem is for the base material.


On Wed, Jun 23, 2021 at 9:42 AM Vishwas Keskar <vvkeskar123@gmail.com> wrote:
Carry out PMI of Weld metal.
If it is welded with E8018 C3 ,PMI will show Ni % .
Take further action as the case may be

On Wed, 23 Jun 2021, 10:36 mohit aggarwal, <aggarwalmoh@gmail.com> wrote:
Hi Experts, 

Hope you are doing well!

We have one problem arises on construction site of material mix-up without any physical traceability i.e. In LTCS line some pipe supports welded of CS material SPS-F-8001 or Structural Material S275 JR but welding done with LTCS 8018-C3 consumable.

Line service is Pressurized LPG with MDMT -45 deg C. material of pipe-SA333 Gr6.

My query is how this can be sort out as client raise the objection of traceability.

Regards
Mohit Aggarwal.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/85cddfa3-0212-4c84-9a8c-fe16ee733576n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/CFm4UP4ukHk/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3NeV2VaNa_KHGT%2Bx1KnhAwjZQLNGDRwRCo_1wQJ%2BB_JFg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOf2ac5A79fAhr2pdqyinDP_5fZHBZMrmPK1i%3D31z6k_cWqo6Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3Pt%3DjE1eeMAS%3DgaesqvaTv%2Bvp_8yZT6zbcBnLjF2O6_hA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...