Re: [MW:32415] Bend Test Jig / Mandrel requirements for Aluminum

 AA 6061-T6,  P.No.23 as per ASME Sec IX.
Pl. inform  % elongation of this material .

On Thu, Jun 3, 2021 at 5:26 PM Prem Nautiyal <prem.nautiyal26@gmail.com> wrote:
Dear All

We need to conduct Face bend and Root bend test for AA 6061-T6,  P.No.23 as per ASME Sec IX.

Thickness of PQR test coupon is 10mm.

We have machined face bend and Root bend specimens with following dimensions  - 300mm L × 38mm wide × 10mm Thick.

Can anyone explain what will be the Test jig / Mandrel dia. as per ASME Sec IX , QW 466.1.
For eg. In steels it is 4T.

Regards

Prem Nautiyal

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEP2HKA%3DOBtRN612TD-kaMHXtEyNZB72-g-qVigdXXLa2bWc6A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3Mwb%2B7aEwscvN8PZ7XeHQZ8ezfNAu_MAohdT8GSOh9SkA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...