Dear Mr Mohan,
Refer Sec VIII DIV 1 UG-102 Test Gage.
Best Regards,
Jay Poojary
On Sat, Apr 28, 2018, 9:17 AM Mohan <ggnanamalli@gmail.com> wrote:
Dear Experts,--Where in the code book does it state that the Hydrostatic Gauge should be between 1.5-4 times for hydrostatic test pressure?RegardsG.Mohanraj
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments