Re: [MW:27665] ASME b 31.3 ,10 % RT means only in total quantity of weld or each welder and line number wise plz advis

Hi

Normally radiography percentage is based on the piping class.

Discuss with the Client representative and finalize.


With Kind Regards

P Govindan 

On Tue, Apr 10, 2018 at 1:42 PM, aravind <aravind.qinspec@gmail.com> wrote:
plz let me know , if design says 10 % RT means only in total number of weld joint or 10% in each welder and line number wise.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...