Hi Manoj,

Normally in API 650 tanks water test is done to analyse the settlement
& to check leak too.

if the tank internal & external is painted, it may mask any possible
pin-holes or cracks etc..

So i personally feel that it is better to do before painting. however
expecting experts

opinion on this as well.


Regards,
Sunil kumar

On 4/23/18, pkkanishk2006@gmail.com <pkkanishk2006@gmail.com> wrote:
> Hi Manoj ,
>
> Yes its possible and ok to do a water fillup test after painting , but pls
> ensure that the painting has been given required curing time to avoid any
> cohesive disbandment .
>
> Regards,
> Pratish
>
> On Monday, April 23, 2018 at 3:52:28 AM UTC+1, John Manoj wrote:
>>
>> Dear expert.
>>
>> We have one proposal to do water fillup test after internal and external
>> painting of water tank which is fabricated as per API 650.
>> Internal paint : 300 micron polyamine cured novolac epoxy coating.
>> External : 205 micron paintining.
>>
>> Is it possible to do water fillup test after painting,
>>
>> Thanks in advance,
>> Manoj.
>>
>>
>>
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> Visit this group at https://groups.google.com/group/materials-welding.
> For more options, visit https://groups.google.com/d/optout.
>

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...