Re: [MW:27717] DISBONDING qualification test for overlay of Cr-Mo STEELS

Follow ASTM G146 for hydrogen disbonding test.

On Tue, 17 Apr 2018, 12:49 Ali Asghari, <asgharialigl@gmail.com> wrote:
Dear All.

Why in API RP934(CLAUSE 7.5.3.2 table 3,4) for simulating domain, doesn't mention to medium as a source of Hydrogen?

Regards. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...