Dear Saumey , 

You have to specify your requirments to PWT to carry out the test and they will be done . They are using Hobbart for your project ?. But tell them clearly about the requirment . If client agrees you carry out the testing but as per ASME sec II part C EQT should be carried out on a plate 1G position . Your production will be J-Groove and extracting specimen for CTOD and all weld tensile will be problem. You have to run a trial in pipe with V grrove which is a pain and I did that . So better demand PWT for EQT records as per your project spec .

On Tue, Apr 10, 2018 at 10:08 PM, Abhishek Vyas <vyas121@gmail.com> wrote:
Since it is a solid wire, for electrode qualification test (Eqt) you can do it by following ASME section II part c

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--

Best regards,

TDK YOKESH

PH : +917092847368


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...