Re: [MW:27727] Distance between two L-Seam

Storage tanks has limitation like below in API 650:

 "Vertical  joints  in  adjacent  shell  courses  shall  not  be  aligned,  but  shall  be  offset  from  each  other  a  minimum
distance of 5t, where t is the plate thickness of the thicker course at the point of offset. "     

which is not applicable in real since results flat spots.



Also

EN 13445-4:2009

6.2 Vessels or parts made of more than one course

Where a vessel or vessel part is made of two or more courses the longitudinal weld joints of adjacent courses shall be staggered by 4 e with 10 mm minimum, or 30 mm minimum when the vessel or vessel part is either working in the creep range or designed by Design by Analysis – Direct Route (Annex B of EN 13445-3:2009) or designed using 6.3 of EN 13445-3:2009.




2018-04-19 7:10 GMT+03:00 'Rajesh Kasvala' via Materials & Welding <materials-welding@googlegroups.com>:
Pl refer uw9 D


On Thu, Apr 19, 2018 at 9:34 AM, udaya bhaskar
My dear, distance between two L seams for pressure vessels minimum 250- 300mm.

On Mon 21 Mar, 2016, 15:57 Ritixa Tandel, <ritixatandel11@gmail.com> wrote:
HELLO,

I AM STUDYING & REFERRING ABOUT DESIGN OF EQUIPMENT. 

CONTINUE TO YOUR DISCUSSION ABOUT ''DISTANCE BETWEEN TWO L-SEAM''........

WHAT SHOULD BE THE MINIMUM DISTANCE IF MY REACTOR IS LIKE THIS:

--SS 316 L REACTOR (3 KL WORKING CAPACITY)
--SHELL: 1500 MM ID x 1700 MM LG x 8 MM THK
--REACTOR WITH DOUBLE LIMPET COIL.

REGARDS RITIXA.
ANKLESHWAR, GUJARAT. INDIA.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7750e6fe-212b-40ed-945e-9d1d8b6c309f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--

Saygılarımla / Regards


Tuğrulhan ÖZDEMİR

API 653 AI, Welding & Materials Eng.

ASNT VT, PT, MT, RT L-II

+90 539 747 2676


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

1 comment:

disha said...

Nice articles and your information valuable and good articles thank for the sharing information limpet coil

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...