There are lot of Factors involved in Radiography to determine the Density Variation for the ID penetration depth. Moreover you use a Double wall viewing and it is very difficult to determine.

Other methods include

1. Boroscopy
2. Ball run Test. A steel ball with the required diameter shall be passed through the tubes and determine the depth of penetration.

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Wednesday, January 31, 2018, 2:52:31 PM GMT+4, 'Sankaran Sp' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Dear Experts,

During pipe to pipe welding by single V butt joint by GTAW process (example : 1" XXS P91 pipe), there is a weld reinforcement over the groove and maintained 2 to3 mm of height, such a way ID penetration is also there. How much of height ID penetration is allowed? which is to be checked by RT exam. Kindly clarify and give me any supporting/ document  reference.

Regards, 

Sankaran.SP
Welding & Metallurgy expert
Coimbatore, India

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...