Dear Experts,
pipe grade is IS 2062 (20" OD x 20mm WT) procured from ex-stock vendor.
Please refer the attached photographs. Crack / Sliver type defect observed near welds and near pipe ends after abrasive blasting.
I do not have more data on the pipe.
What may be the reason for this defect.

--
Thanks and Best regards

M. Vinod Kumar

"Never Explain yourself to any one Because the person who likes you doesn`t need it, and the person who dislikes you won`t believe it."

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...