Re: [MW:27256] Aluminum welding 6061-T6 mechanical test bend failure

Go for pwht first solutinizing bring material to T4 condition then artificial agening to meet T6 condition for entire structure

After welding weld haz & parent metal all should be in same ageging condition to reduce craking

--