Dear Sir,

As per the NACE requirement 7.3.3.3 of doc MR 0175, indicates requirements for hardness survey of PQR [WPS qualification] test on different weld joint types. A PQR coupon of Fillet only needs hardness survey as per FIG 3.

But you are using a WPS qualified with butt weld, hardness tested per NACE. This qualified WPS may be used for doing production weld of fillet. ASME SEC IX permits the qualification by butt weld qualifies for fillet weld also.

Hence the same procedure can be used for production weld - fillet.

Regards,
MANIVANNAN.P



On Fri, May 26, 2017 at 6:58 PM, Baskaran <baskaran.avc@gmail.com> wrote:
Dear Experts,

Please advise on below query.

Applicable code are;
ASME Section IX
NACE MR 0175.

We have one WPS Qualified in butt joint and Hardness survey done  according to NACE MR 0175 (7.3.3.3 Figure 2)  on Butt weld coupon.

​Is it correct that we cannot use the above WPS in a fillet joint because the fillet weld hardness survey is not carried out.

​Thanks.​
Bas

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...