After I ask this question here and can't get any answer for a long time, i ask some of our customers experts and here is the answer: 

According to 15614-1 Clause 8.4.4 Same group of the wires cover each other. 

with this like your answer, if the consumable wire class according to standard not changed, I can use whatever I want without any new test coupon.

but if I want to change the root wire, I need to prepare a test coupon that covered the root weld thickness and combine two PQR to create a new WPS (According to EN 15614-1 Clause 8.4.1).

Thank you for your answer. 

These are the official answer i get from customers welding expert. 

Regards. 

31 Mayıs 2017 Çarşamba 13:00:33 UTC+3 tarihinde UtreWeld yazdı:
In my opinion, if they have the category of wire2 is the same than category of wire1 they could be exchanged.

Regards,

El martes, 23 de mayo de 2017, 10:21:10 (UTC+3), uguruzar escribió:
the root wire on PQR1. 

but I don't want to make complete test. 

On the PQR1 i used root wire1; and i want to make a new test with only root wire2 with same thickness range on PQR1 root thickness.

can i use these two PQR tests to create new WPS described on the sketch.

Regards. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...