Dear All,

Referring to API 650, Section 5.7.3.1, is it correct to conclude that no stress relief is required for shell plate to shell plate weld joints (having shell thickness 36 mm, material SA 537 Cl II), if following conditions are met:


1. Minimum spacing requirements mentioned in section 5.7.3.1 (a) are met- We are maintaining minimum 300 mm distance for dimensions mentioned as A and B in figure 5.6.

2. Minimum spacing requirements mentioned in section 5.7.3.1 (b) are met- We are maintaining minimum 300 mm distance for dimensions mentioned as E in figure 5.6.


This tank is a existing tank, we are adding few nozzles for mixers and for process inlet.


Appreciate your response on the subject.


Thanks in advance. 

Regards,

Rajnish

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...