Monday, May 22, 2017

Re: [MW:26529] Acceptance criteria as per B 31.3

Dear Sir

You have to evaluate the cumulative length of incomplete penetration but also the depth (≤ 1 mm (1⁄32 in.) and ≤ 0.2Tw), according to table 341.3.2.
As it is not possible to verify the exact depth of the incomplete penetration (talking about RT interpretation) and if the contrast of film is clear, i usually do not accept more than 5-10mm cumulative length in M category fluid. Again, the code has defined minimum acceptance level.

Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...