[MW:26529] Multi Process Qualification (MAG+SAW)

Hi.

I have question;

I have a PQR for multiprocess (root: MAG, filler and cap: SAW)

I want to change root wire only.

If i make a test for just root thickness with new wire can I combine with these two PQR for a new WPS?

I tried to explain with a sketch below.

(According to EN 15614-1 Clause 8.4.1)


FotoğrafThanks in advance. 

--