Sockolet is a fillet weld. See QW-451,3 or QW-451.4 for the WPS qualification.
If the welder was qualified by means of a groove weld, practically for fillet he can weld any thickness (see QW-452.6)
However beware of the diameter qualification range
-- If the welder was qualified by means of a groove weld, practically for fillet he can weld any thickness (see QW-452.6)