RE: [MW:26142] ASME code for fuel piping

GHRAB Zakaria,

 

ASME B31.3 is for process pressure piping (e. g. petrochemical)

ASME B31.8 is for gas transmission & distribution piping systems (e. g. natural gas)

 

Dennis Thompson,

TeamQualspec

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zakaria ghrab
Sent: Tuesday, February 28, 2017 11:40 AM
To: materials-welding@googlegroups.com
Subject: [MW:26140] ASME code for fuel piping

 

Dear experts,

 

  Could you advice about the ASME construction code for Fuel piping. 

From B31 serie i suppose

 

Thank you.

 

--

 

Thanks and Regards, ?

-----

زكرياء غراب
GHRAB Zakaria 



Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD8EeB3Apqgpv5q-L2SKyVtxv9qjmt7dxOcNTtSahbXbTmgiNA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...