Friday, March 31, 2017

Re: [MW:26329] Circumferential pipe weld joint resting on structural beam in process piping

Generally,  piping drawings shall take care of this type of issues during fabrication of pipe spools. 

It is a very common problem, if you don't have any option to move the support,  then before the support cut and add one pup piece pipe and do all welding and NDT as per the  regulations  and avoid the fouling. 



Regards
Anil 

On Mar 28, 2017 8:51 PM, "'Biplab Pal' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Dear experts,

We need your kind support based on your experience and any code/std references.

The situation is that some of our process piping in refinery division THE CIRCUMFERENTIAL JOINT has come such position that the joint rests on the structural beam.
Is it allowed?

Some inspector have a concern that there is a developed stress while operation and the joint may fail.

Please share your experience and reference.

Thank you very much 

With best regards
Biplab Pal
--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnzQg22xWSiTOEonpZtZCDqBZ9vvh9OGZ_bKvHJ9CrS1L-qSg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK2QV3T7Pyq%2BfEEFBQDrGLvUUzKY90gEVqU1zaH5erqXjjHqmg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...