[MW:26243] RE: 26238] Shielding gas for GMAW pulsed welding-Carbon Steel

Hi Aby,

 

More enriched version of mixed gases, e.g. 90Ar+10 O2 or other Ar enriched blends may help. Look at this guide ,which has few  good recommendations about shielding gases.

 

Thanks.

 

P.Goswami,P.Eng,IWE.

 

https://www.lincolnelectric.com/assets/global/products/consumable_miggmawwires-superarc-superarcl-56/c4200.pdf

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Aby Jose
Sent: March 21, 2017 4:56 AM
To: materials-welding@googlegroups.com
Subject: [MW:26238] Shielding gas for GMAW pulsed welding-Carbon Steel

 

Dear all,

 

What shielding gas should be used for the pulsed GMAW welding of carbon steel? When trying with 80%Ar+20%CO2 mixture I am getting a lot of spatters. The welding used is Automatic welding with Robotic machine.

Any recommendations???

 

Regards,

Aby

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACdTRdyc8NMn6LBHHHTeYFxP_Ani0cnWDw0j5qEJSyRyfoOe4Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...