A 20% carbon di oxide mix in a 80% argon usually works best in spray transfer mode in w position so you would need to ensure that you aren't using short circuiting mode which is resulting in large amount of spatters. In case you're welding thin sheets or doing out of position welding you may have to consider changing the gas mixture
Trust this helps
Sent from my iPhone
Sent from my iPhone
Try for 98% argon and 2% co2--
On Tue, Mar 21, 2017 at 12:56 PM, Aby Jose <abycscec@gmail.com> wrote:
Dear all,--
What shielding gas should be used for the pulsed GMAW welding of carbon steel? When trying with 80%Ar+20%CO2 mixture I am getting a lot of spatters. The welding used is Automatic welding with Robotic machine.Any recommendations???
Regards,Aby
http://www.linkedin.com/groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
To post to this group, send email to materials-welding@googlegroups.com .
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ .CACdTRdyc8NMn6LBHHHTeYFxP_ Ani0cnWDw0j5qEJSyRyfoOe4Q% 40mail.gmail.com
For more options, visit https://groups.google.com/d/optout .
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEML-XRowcwexs%3DZz4xzozQA7Q6p6XcbJr1YNpG98vBsr-o90w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments