Try for 98% argon and 2% co2
On Tue, Mar 21, 2017 at 12:56 PM, Aby Jose <abycscec@gmail.com> wrote:
Dear all,--What shielding gas should be used for the pulsed GMAW welding of carbon steel? When trying with 80%Ar+20%CO2 mixture I am getting a lot of spatters. The welding used is Automatic welding with Robotic machine.Any recommendations???Regards,Aby
http://www.linkedin.com/groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
To post to this group, send email to materials-welding@googlegroups.com .
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ .CACdTRdyc8NMn6LBHHHTeYFxP_ Ani0cnWDw0j5qEJSyRyfoOe4Q% 40mail.gmail.com
For more options, visit https://groups.google.com/d/optout .
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEML-XRowcwexs%3DZz4xzozQA7Q6p6XcbJr1YNpG98vBsr-o90w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments