[MW:26283] Re: Welding repair procedure required. (ASME or AWS)

Dear Ghani,
Repair. In the repair and determination of
limits of mill induced discontinuities visually observed
on cut surfaces, the amount of metal removed shall be
the minimum necessary to remove the discontinuity or to
determine that the limits of Table 5.4 are not exceeded.
However, if weld repair is required, sufficient base metal
shall be removed to provide access for welding. Cut surfaces
may exist at any angle with respect to the rolling
direction. All welded repairs of discontinuities shall be
made by:
(1) Suitably preparing the repair area
(2) Welding with an approved low-hydrogen process
and observing the applicable provisions of this code
(3) Grinding the completed weld smooth and flush
(see 5.24.4.1) with the adjacent surface to produce a
workmanlike finish.
Note: The requirements of 5.15.1.2 may not be adequate
in cases of tensile load applied through the thickness of
the material.

Thanks with Regards'
Atif Aslam (Din).

On Tuesday, January 5, 2016 at 1:19:32 PM UTC+6, Ghani wrote:
Dear Expert,

I need welding repair procedure for structures, were can i find standard repair procedure (ASME or AWS).

Kindly guide for the welding repair procedure for structural welding


Regards

--
Thanks and Regards, ?

Mohammed Ghani,

CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.
Mechanical Inspector,
ü Please consider the environment before printing this email.

 "Be the change you wish to see in the world"

---Mahatma Gandhi---

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9d712afd-ebd6-4a40-a9d5-375bdbef99b3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...