Pressure test is a mandatory requirement of  pressure piping designed and fabricated according to B-31.1 code. Clause 137 & various other clauses  of this code explicitly specifies the requirements. The medium could be Hydro or Pneumatic.

 

Pneumatic test is  not advisable for safety and integrity of piping components. Hence Hydro test is the default choice.

 

Hope it clarifies your doubt.

 

Thanks.

 

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical  Engineering Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

 

 

From: Ganesan [mailto:ganesandme03@yahoo.co.in]
Sent: March 30, 2017 7:25 AM
To: materials-welding@googlegroups.com; PGoswami <pgoswami@quickclic.net>; materials-welding@googlegroups.com
Subject: Re: [MW:26315] RE: 26313] Hydro Test

 

Noted for your valuable point. But the contractor is asking to show the code requirements. 

 

B31.1 has followed for design and fabrication of the Piping. 

 

 

On Thu, 30 Mar 2017 at 12:21 p.m., PGoswami

<pgoswami@quickclic.net> wrote:

What's the design and fabrication code for Piping??

 

Usually pressure piping  have to be hydro tested (by default) as like pressure vessel. No exceptions to rules?

 

A citation from the appropriate code or mentioning the appropriate code would be appreciated.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Welding&Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

From: 'Ganesan' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Sent: March 29, 2017 6:13 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:26313] Hydro Test

 

Dear Experts,

 

Could you please share the standard requirements for piping hydro test, because our chines contractor has not ready to conduct hydro test for the same piping. they said as per chines standard no need hydro test.

 

  

 

Thanks & Regards, K.GANESAN Quality Control ISGEC / ISGEC John Thompson, A-4 Sector-24 Noida-201301 (UP) Tel. +91-120-2411175 Direct Tel. +91-120-2411175 Mobile : +91-9952166894

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1216733524.5643000.1490782373350%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

 


This email has been checked for viruses by AVG antivirus software.
www.avg.com



--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAB/s9XS594ZCoMHlmX4xaZ3CgAAAEAAAADNg4iY9mnhIoxuiarCDI9UBAAAAAA%3D%3D%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...