Saturday, February 11, 2017

Re: [MW:26040] Filler wire for welding SA 240 TP 304 to SA 276 TP 310 Mateial

309ok and 310 only( 347 stabilised one)

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sat, Feb 11, 2017 at 1:07 PM, GALAXY INDUSTRIES PRASHANT PANCHAL <pipanchal@live.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (pipanchal@live.com) Add cleanup rule | More info

can we use ER 309 filler wire for welding SA 240 TP 304 to SA 276 TP 310.


& ER 347 filler wire for welding SA 276 TP 310 to SA 276 TP 310.


Regards,

Prashant Panchal


From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of Kannayeram Gnanapandithan <kgpandithan@gmail.com>
Sent: Saturday, February 11, 2017 12:33:33 PM
To: materials-welding
Subject: Re: [MW:26038] Filler wire for welding SA 240 TP 304 to SA 276 TP 310 Mateial
 
308 and 310

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sat, Feb 11, 2017 at 12:14 PM, GALAXY INDUSTRIES PRASHANT PANCHAL <pipanchal@live.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (pipanchal@live.com) Add cleanup rule | More info

Dear all,


Kindly let me know the filler wire to be used for welding SA 240 TP 304 to SA 276 TP 310 material & SA 276 TP 310 to SA 276 TP 310 Material


Thanks & Regards,

Prashant Panchal




http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/D9EA8DC3-B050-49CA-8706-B751739B0B3C%40yahoo.com.
Google Groups allows you to create and participate in online forums and email-based groups with a rich experience for community conversations.


For more options, visit https://groups.google.com/d/optout.
Google Groups allows you to create and participate in online forums and email-based groups with a rich experience for community conversations.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BL2PR17MB0833E556E9F0809143B645C4C3470%40BL2PR17MB0833.namprd17.prod.outlook.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePTL0HcNS4Z3qTa64cO%3Dw27WjkFke3KSE%3DsRskfWWgKSA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BL2PR17MB08336C44D3CE01CD635A9FE8C3470%40BL2PR17MB0833.namprd17.prod.outlook.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNQt_%3D1Pcs1OafDgc3Zz7aoK3_WuUyDPd7%2BhFGgaNWSpw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...