Re: [MW:26100] is required new PQT for repair PWHT

I would recommend that you read carefully UCS-56 (f) in ASME Section VIII-1 

2017-02-17 8:57 GMT+02:00 sid <sjawale61@gmail.com>:
hi 
i am using A 106 Gr B material P-1 material (GTAW+SMAW) and WPS is qualify with PWHT 
if weld joint repair after PWHT shall can proceed with new PQR
sec IX 407.2 is given new qualification required for if any changes in Time and thickness
please reply 


Siddharth 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9a154f58-0e8d-482b-bd4d-026503035e1f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CMY2E%2B9xa54di3N4Fv%3DJ_4L2JiYnw0gXGOiOut3%2BDFxg%40mail.gmail.com.