Monday, February 27, 2017

Re: [MW:26132] Can we use S355J2+N instead of ASTM A36

Dear ,

Generally S 355J2 is not getting accepted, If available you  go with s275 grade,as listed in ASME 9, P1G1.

*DINESH VITTHAL SOMWANSHI*

*BACHELOR IN MECHANICAL ENGINEER*

*AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL,*
*API 570 - Piping Inspector,** AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3*
*NDT II -UT , RT , MT , PT, VT*
00919881344135
Skype = dinesh570_1

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*


On Mon, Feb 27, 2017 at 10:42 AM, Lalit Malla <lalit.malla@gmail.com> wrote:
Dear All,
Can we use S355J2+N plate instead of ASTM A36 plate for pipe support fabrication. In my opinion, S355J2+N is higher grade steel but will there be any problem with client acceptance ?
Your immediate response shall be highly appreciated. Thanks

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5e3de2f7-9b2d-43fb-a3ad-1c2be2431662%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrXw7TjPbGe-zKeuJEB01RoUGUw%2B7-Nzj%2Bf31OxueN8Ozg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...