Monday, February 27, 2017

[MW:26137] Re: NER and Vacuum for cryogenic tank

Hi M. Georgios Dilintas,

Thanks for your replay.

I correct, Evaporation not Evaluation

For help, I need your experience about the Evaluation of NER by pressure rise methode.

Your response for my preocupation is helpful.

Thanks in advance.

Benadjal Redouane
Mechanical engineer Sonatrach algeria

Le lundi 20 février 2017 10:45:43 UTC, Brl Pp a écrit :

Good morning every body,

Following your knowledge and your experience, please advise me how to determine the nitrogen evaluation rate (NER) for the cryogenic tank.

My question:

-          Is there any code to control the NER?

If no code any procedure or specification on the subject would be appreciated.

Also, following the Manufacture's Data Report for the tank, the acceptance standard maximum is 150 mtorr for 72 hours. Is this value (150 mtorr) mentioned in the codes and standard or just manufacturer's standard?

Thanks in advance.

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/97bd4ecf-4874-4270-8324-84d098690cb5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...