6013 is having Hydrogen level of >15<30PPM and if it is used in higher and multi-layer welding, there is lot of change for HICC, so it is restricted for thickness below 13mm

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Thu, Feb 16, 2017 at 2:08 PM, Raju Kandula <rgkandula@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (rgkandula@gmail.com) Add cleanup rule | More info

E 6013 electrode was primarily designed to provide good wetting and shallow penetration for thin sheet metal applications and E7018 provides medium penetration

On Sun, Oct 30, 2016 at 5:34 AM, Prasad Rode <purode333@gmail.com> wrote:
Dear sir,

As per API 650, above 12mm E7018 has to be use. Means up to 12mm E6013 has to use.
I have only query to ask that, why e6013 not allow to use above 12mm.


Regards
Prasad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9d470b07-b7e7-4fd5-a607-4a65202d869e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALwNT%2B-TGn2rSSuAcJcjVd5hVEzAVVU_yzF8Uv18d5NBBGsXHA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePPrxrFLzBkR7Hvy_65AKXh7p4qT3T_v5DH0mW6vbcaug%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...