Re: [MW:26064] Welding of Low alloy to Stainless Steel

What is thickness?. If it is less than 13mm, u can directly weld. If thickness is greater than 13mm, buttering and sr to be done on P5A side and then weld with P8


On 13-Feb-2017 4:54 PM, "pradip kumar Sil" <pradipsil@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (pradipsil@gmail.com) Add cleanup rule | More info

It is better to do Buttering.

On Mon, Feb 13, 2017 at 9:38 AM, Shaunak Upadhyay <shanupadhyay@gmail.com> wrote:
Dears,
 
Please give your valuable guidance.
 
I have weld joint between P5A to P8 materials, using nickel base consumable.
Before start this butt joint, is it mandatory to do buttering on P8 material ? or we can weld direct butt joint groove between these two materials. (SA387 GR22 CL2 or SA240 TP304L)
 
Thanks, 
Regards,
Shaunak Upadhyay.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD1AzTQxzQDMfnMr1%3DKJO8uYa8vQN-Ep_pn1Lh9torEHLsLEsw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8k-jBE2MXP6vg4LTscu1OhCqU4D2j_zj1BYcVk5APBrqw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNmvNzqFM-GERiB6N34cjk3m0sdyVdmiXue7tLAu6WKXQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...