Dear Sir,

As we all of us known too and always talking about mild steel and carbon steel material.

As I know that, carbon percentage makes a difference to differentiate carbon steel and mild steel. As mild steel has low carbon percentage as compared to carbon steel.

But I want to know that as carbon steel comes in IS2062 category, then mild steel has to be study by which code?

Or
if we say IS 2062 for mild steel plates, then we can concluded that grade C is mild steel while grade A is carbon steel. Is it right.

Basically, I want to know, above which carbon % , material is said to be carbon steel and below which mentioned as mild steel.
In which code or standard it is mentioned?

Regards
Prasad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2a6eecdb-0172-4107-9ffe-2cd302712759%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...