Hi S355 J2+N is much than A36, and your client is likely to accept your substitution
-- On Mon, Feb 27, 2017 at 1:21 PM, Lalit Malla<lalit.malla@gmail.com> wrote:Dear All,--Can we use S355J2+N plate instead of ASTM A36 plate for pipe support fabrication. In my opinion, S355J2+N is higher grade steel but will there be any problem with client acceptance ?Your immediate response shall be highly appreciated. Thanks
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5e3de2f7-9b2d-43fb-a3ad-1c2be2431662%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1852451257.1889881.1488186680495%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
Comments