[MW:25469] Weld Overlay Profile acceptance Criteria

Dear All 
Pls find attached herewith the photograph of Weld Overlay On ID of Nozzle 3'' x 500mm Long.
The attached Photo showing Irregular Profile which is Visually not Acceptable.

As per our argument with QC manager of one of the Co. asking me what is the difference between smooth and rough profile and why this is not acceptable.

As Per ASME Section VIII weld should be smooth and free from cores ripples, ridges.

Could you pls anybody reply for the same?    

--
Israr Ahmed Noor Mohammed
+919930308261

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEJozaKs07rbRmRrSo6aVBhh7wjeq1BB1Sph8edWfqYnBz%2BfMg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...