Re: [MW:25545] Weld Overlay Profile acceptance Criteria

In weld overly ripples are common. Go with PT examination (solvent based), if the examination shows indications. Then u can reject it. If the penetrant gets easily removed and doesn't show any indications you can accept it. 

Sent from my iPhone

On Oct 10, 2016, at 10:41, Venkatesan Velayudam <velvenkat2002@gmail.com> wrote:


Dear Ahmed,

You have not mentioned the required thickness of weld overlay.

Weld overlay on ID of Nozzle 3'' x 500 mm Long is very difficult to weld. 

So to get better weld profile after weld overlay you need to do machine the nozzle ID to required thickness.

You can adopt UT for check the weld overlay thickness.


Regards

Venkatesan





 


On Fri, Sep 30, 2016 at 10:37 PM, israr ahmed <ahmedisrar.nm@gmail.com> wrote:
Dear All 
Pls find attached herewith the photograph of Weld Overlay On ID of Nozzle 3'' x 500mm Long.
The attached Photo showing Irregular Profile which is Visually not Acceptable.

As per our argument with QC manager of one of the Co. asking me what is the difference between smooth and rough profile and why this is not acceptable.

As Per ASME Section VIII weld should be smooth and free from cores ripples, ridges.

Could you pls anybody reply for the same?    

--
Israr Ahmed Noor Mohammed
+919930308261

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEJozaKs07rbRmRrSo6aVBhh7wjeq1BB1Sph8edWfqYnBz%2BfMg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABgMRAUB-fs9wfZHdoC4T7bVqJ422x_ogSG8ZCWoEE%3DZtFB6eg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...