Dear vikas,
You have to qualify welder in 2 inch to weld that weldolet on 24 inch pipe....
Regards,
Vivek
On 15-Oct-2016 5:50 PM, "Vikas Waghmare" <vikas.waghmare08@gmail.com> wrote:
Dear all,
I want to weld 2inch weldolet to 24inch pipe, my doubt can i use welder qualified as per section 9 with diameter range 73mm and above to weld 2 inch weldolet whose OD is above 73mm.
Second doubt how much weld i need to deposit on weldolet to run pipe connection if code of construction is asme B31.3, i think it should be minimum thickness of branch or run pipe thickness and then make fillet. Or is it needed to deposit weld upto bevel end then a fillet.Regards
Vikas
--
http://www.linkedin.com/groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
To post to this group, send email to materials-welding@googlegroups.com .
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA% .2BCgecnc- uScigVNxcd15GJQmb8ZhT- SWKO2eoFX%2BJhg7%2Bkpyw% 40mail.gmail.com
For more options, visit https://groups.google.com/d/optout .
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFOZxBj6SVzj%2B7RFXREdsRGSqgM_5Xm2MvR8Dr3Z9O-sD0gr2w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments