To all,
-- The new EIL spec prescribes PWHT to be performed for all CS materials used for sour service irrespective of the thickness..
Is it required to do PWHT for all joints(1",2",4",6" etc) for CS Nace based on this spec??
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---