Re: [MW:25595] Storage Tanks (API-650) Settlement Reading Range



 


Dear Meghanadh k,


Thank you,


No, it is not in-service plant its a new Refinery project we are required to fabricate and erect new storage tanks according to API-650. 

 

Regards,

 

Akmal Malik.

 
 



From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of dilintas <dilintas@gmail.com>
Sent: 25 October 2016 00:13
To: Meghanadh K
Subject: Re: [MW:25594] Storage Tanks (API-650) Settlement Reading Range
 
It is an in-service inspection? Then better look on API 653



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Akmal Malik <akmalm72@hotmail.com>
Date: 25/10/2016 14:07 (GMT+02:00)
To: materials-welding@googlegroups.com
Subject: [MW:25592] Storage Tanks (API-650) Settlement Reading Range



 

Dear Experts,


I need your option and advice regarding Tank Survey Settlement, As specified in API 650, clause # 7.3.6.5 (2). This clause refers “Observed elevations shall be referred to a permanent bench mark. The level instrument shall be set up at least 1 ½ times tank diameter away from the tank when tank elevation readings are taken”

Practically it looks impossible, if the tank diameter is more than 60 matters. We have 68/72/84 and 106 diameter tanks in our scope of work, I participate with our surveyor team for the settlement survey, if we are  1 ½ times tank diameter away from the tank the reading or result can’t be accurate. Yes if we are near to tank like 20 to 30 meters away from the Tank than found all settlement reading accurate.

Our client insist to maintain the distance according to API 650, clause # 7.3.6.5.even the required distance range is outside the dike wall.

 

Please advise.


Looking forward to you,


Thanks& Regards,

Akmal Malik

Jazan-KSA



 

 


 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/v9908362nf6kvae01q387yjg.1477397631292%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...