Dear Shaik,

Please note that S355J2 or JR Materials are unassigned materials without P nos, so you have to qualify with the actual base material in this case.
However you can approach the clients by saying that the yield strength is same and the consumables used also will be same, in that case may be they will accept.

On Mon, Oct 31, 2016 at 2:50 PM, shaik amjad <amjadshaik7842@gmail.com> wrote:
If a wps is qualified in base metal S355J2 will it be qulified for S355JR Code AWS. I have WPS qualified with base metal S355J2  but now due to stock availability only S 355JR is available can i use same WPS for this one also . as only the grade is changing  

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/288c4978-e27c-4ec3-abac-5ae1f4cb7f53%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp9iEnrEBWwQ%3D_Kb6%2BYN%2BGqt%3D4vj8Xbm7NPREK9Ku593_A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...