You may say to your client that in the frame of PED for welding consumables 2.2 certificate is acceptable. 
Further more in the frame of BPVC ASME welding consumables are accepted on the basement of marking and no material test report is required 



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Kumar <sk7920541@gmail.com>
Date: 21/10/2016 13:30 (GMT+02:00)
To: materials-welding@googlegroups.com
Subject: [MW:25581] 2.2 & 3.1 MTC

Dear Experts,

Greetings.

Requesting the views on MTCs (EN 10204 ) for electrode  ( SFA/AWS A
5.1 E 7018-1 H 4 R, 4.00mm). In fact according to project spec. it
should be 3.1. but the contractor could only provide 3.1 for chemical
& mechanical 2.2 in a single MTC.

Since its a deviation from the spec., how far this will affect the
quality of the product when mechanical according to 2.2 & chemical
according to 3.1? how this could be convinced to the end user.

Your valuable feedbacks are appreciated.

thanking in advance,
Kumar.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALuBtp9j4g08J_sEsjtQ15OF2%2BUyZh8k1v9ky8arTPB53bbVtA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...