[MW:25554] Re: do we need seperate wps for repair

thank you sir for your reply
if possible can you explain these in the para 328.6"
recognizing that the cavity to be repaired may differ in
contour and dimensions from the original joint."


thank you



On Monday, 17 October 2016 08:20:10 UTC+4, anil kumar wrote:
Hi,

       Do we need separate wps for repair or the wps we used in production will be sufficient as per ASME B31.3,
and using the  PQR which used in production , can I qualify repair wps.

Thank you
ANIL KUMAR

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d5fb69d6-7c9b-4a0d-8ed3-5d6cfeeda7aa%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...