Dear

In my knowledge, As per API 1104 , the welders production becomes questionable, then need review on their qualification. So even after the 3 or 4 months their production is good , they can continue...with out requalification.


Thanks & Regards

PRADEEPKUMAR HORMIS

QC WELDING & PIPING SPECIALIST
SAMREF Clean Fuels Project
P.O.Box 30078
Yanbu Al-Sinaiyah 41912
Kingdom of Saudi Arabia


 







On Thu, Jun 26, 2014 at 2:44 PM, Richard robes <mech.processes@gmail.com> wrote:
if your welders are not working upto 6 month's then its required to requalify, otherwise as in your case welders can just proceed without requalifying unless specified by the client.


On Sat, Jun 21, 2014 at 9:58 PM, LALU RAJENDRAN <lalucpt@gmail.com> wrote:
Dear Zakaria,

It depends upon your Client.If your client suggest you to do that, you can convince them or else provide them with the recent NDE reports if they are working in some other projects.



On Thursday, June 19, 2014, Malusare Vijay <vijaymalusare07@gmail.com> wrote:
Dear GHRAB Zakaria
 
as pe code it is not required but if client say that then you have to do same because client above the code.
 
Regards,
 
Vijay Malusare

On Wed, Jun 18, 2014 at 11:29 PM, Zakaria ghrab <zakaria.ghrab@gmail.com> wrote:
Dear Experts,

  We have one pipeline project according API 1104. Now with agreement
from us and client will stop all welding activities and restart after
03 or 04 months.

My request is: Will continue work with our welders but i don't know if
is it mandatory to retest, some renewal qualification ... I checked
API 1104 but nothing about this.

Regards.

--
*-----*

*زكرياء غراب**GHRAB Zakaria*
SEME Redeveloppement Project
Geocean - Project QC Engineer
Tunisia : +216 96 635 805
Morocco : +212 6 06 58 88 56
Bénin : +229 97 128 387


Yesterday is the pass, tomorrow is the future; and today? Today is the
present, the gift: Enjoy it!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
Thanks & Regards,

LALU R.P

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...