Re: [MW:21209] QW 406 , preheat maintenance

Always during welding the joint temp has to be maintained between preheat and interpass  temps.
 
With Best Regards,
Shashank C Vagal


On Saturday, 21 June 2014 9:18 AM, "rajesh s. mhaske ,Engineer Welding ,PUNE,INDIA" <rajesh.mhaske17@gmail.com> wrote:



   Dear sir
               thickness and  OD : 323 od* 70 mm thk
               welding process : GTAW+SMAW
               Material : SA106 Gr B
               Preheating : 100 deg c
               weld deposition : for GTAW : 4 mm, SMAW : 66 mm


   Question  :
                  1) Is the preheat maintenance (post heating ) is required for  above material
                  2) If YES, what is time and temp  plz send the back up
    

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...