Re: [MW:21280] gain size of stainless steel of material A 350 LF2 of austenitic grade

Hello,

standard methods of evaluating grain size are mentioned in ASTM E112-10.

On Friday, June 27, 2014, Brijesh Patel <pbrijesh103@gmail.com> wrote:
> Dear Sir,
> my question regarding to gain size of austenitic stainless steel material of  A350 LF2
> 1) how to check gain size of above material?????? 
> 2) what is acceptance criteria for gain size???
> 3) which gain size check Austenitic or ferrite ?????
>
> --
> Thanks & Regard's
>
> Brijesh Patel
> Engineer
> cell no.:- +91 9727013016
> IRCLASS Systems & Solutions Pvt. Ltd.
> (Subsidiary of Indian Register of Shipping)
> 301,302,303, Sakar Complex, 3rd Floor, Old Padra road,
> Malhar Point, Haribhakti Extension, Baroda-390007
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>  
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...