Re: [MW:21256] Post weld heat treatment for blind flange of manhole when lethal service.

Lethal service ,Pwht Required due to more than 13 mm thick fillet size Sec viii table ucs 56 notes 2(c)3.
On 25 Jun 2014 06:13, "ji Ch" <jinsuok21@gmail.com> wrote:
>
> Sir.
>
> I've question for this subject.
>
>
> In the ASME Sec.VIII Div.1, 
>
>
> The vessel fabricated by carbons steel, and it applied lethal service, so it need post weld heat treatment refer to UW-2 (a) 
>
>
> In this case, for blind flange of manhole, davit hinge welded to side portion of blind flange with over 16mm weld thickness of fillet weld.
>
>
>
> is this blind flange also required post weld heat treatment ? or not ?
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>  
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...