Dear sir
Pipe dia : 323.*33 mm thk
Tube dia : 50.8 *6.35 mm thk
Groove design for above pipe to tube welding : set in (groove on header ) / set on (groove on tube )
Welding process : GTAW + FCAW
Qualification of welder: OD >73 mm and Thk - Max to be welded with process GTAW+FCAW
Question :
1) Can above qualified welder be deployed for welding of set in and set on joint.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments