Re: [MW:19141] Re: Change in Supplementary Essential Need re-qualification?

Hi!
 
No, you require to qualify for P1 Gr 2 asGroup no  is suplimentary essential
Regards
Hegde P.B.
 

From: B R Meghwal <br.meghwal@fernas.co.in>
To: materials-welding@googlegroups.com
Sent: Thursday, 31 October 2013 5:14 PM
Subject: [MW:19126] Re: Change in Supplementary Essential Need re-qualification?

Dear All,

Please be informed that we have carried out the WPS & PQR of P No-01 Group no.01 materials with notch toughness test (including HAZ).

With reference to above, Can I establish a WPS of P No-01 Group no.02 materials as per ASME Section IX latest edition???

Your prompt & valuable respond along with details will be highly appreciated.

Thanks & regards,


On Tuesday, 29 October 2013 11:36:33 UTC+5:30, Tiger wrote:
Dear Experts,


i need your clarify that the changes in material group number with the
same p number need another welding qualification or not.

my case i have WPS for A312  grade TP 316, P no. 8 , group no. 1 to itself.
it&apos;s right to use it to weld  A312  grade TP 310s, P no. 8 , group no.
2 to itself.

Ezzat
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group&apos;s bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...